Typical values
| Property | Value | Unit | Test method | Condition |
|---|---|---|---|---|
| All attributes | ||||
| Melt Flow | 3 – 8.4 | g/10 min | IM 1099-A | |
| Speck Size | 0 – 20 | IM 1692 | <= 299 UM, # | |
| Speck Size | 0 – 7 | IM 1692 | 300 - 549 UM, # | |
| Yellowness Index | -99.99 – 10.4 | IM 1103 | ||
| Extrusion Gel Index, Number | 0 – 3.4 | IM 773-B | >600 µ/m² | |
| Mechanical properties (23 °C; 50 % r. h.) | ||||
| Hardness Shore D | 47 – 53 | IM 436-B | ||
| Tensile strength | 12.41 – 15.86 | MPa | IM 453-A | 100% Elongation; 200 mm/min |
| Tensile strength | ≥ 8.97 | MPa | IM 453-A | 50% Elongation; 200 mm/min |
| Tensile strength | ≥ 42.75 | MPa | IM 453-A | at break; 200 mm/min |
| Elongation | 380 – 550 | % | IM 453-A | |
Documents